DIMINISHMENT OF INTERNAL POLYGONIZATION OF TUBES IN HOT STRETCH-REDUCING MILL

Authors

  • Krzysztof Stefański
  • Wiktor Kubiński

DOI:

https://doi.org/10.7494/mafe.2010.36.1.21

Keywords:

stretch-reducing rolling, steel tubes, internal polygonization

Abstract

One of the most important issues in hot stretch-reducing process is the maintaining precision of wall thickness. Exactly the same wall thickness at all cross-sections of tubes after stretch-reducing mill increases suitability of tubes in the next treatment processes. Internal polygonization of tubes and its removal during hot reducing is constantly the most important problem. The study is a presentation of test results for decrease of internal polygonization. Internal polygonization, as a result of deformation of tube wall thickness in all stands during hot reducing, can be minimized first of all by optimization of inter-stand tension. The tubes and pipes with minimal internal polygonization could be obtained during experiments of rolling after applying maximal average tension using a developed system for equations of axial forces equilibrium in the rolling mill.

Downloads

Download data is not yet available.

References

Thieven R: Untersuchungen zur Innenpollygobildung beim Streckreduzieren von Rohren, Stahl und Eisen, (1996) 8, 119-125

Biller H:. Beitrag zum inneren Unrundwerden beim Reduzieren von Rohren, Diss. TH Aachen [3] Kazanecki J. Wytwarzanie rur bez szwu, UWN-D Wydawnictwa AGH, Kraków 2003

Downloads

Published

2010-06-30

How to Cite

Stefański, K., & Kubiński, W. (2010). DIMINISHMENT OF INTERNAL POLYGONIZATION OF TUBES IN HOT STRETCH-REDUCING MILL. Metallurgy and Foundry Engineering, 36(1), 21. https://doi.org/10.7494/mafe.2010.36.1.21

Issue

Section

Articles